Common Defects in LSR Baby Nipple Molding and How to Fix Them

Liquid silicone rubber (LSR) injection molding plays a critical role in the production of baby nipples. The process delivers excellent consistency, hygiene, and performance-but only when manufacturers control materials, tooling, and processing conditions correctly. Even small deviations can lead to defects that affect safety, comfort, and durability.

This article breaks down the most common defects found in LSR baby nipple molding, explains why they occur, and outlines practical solutions from a technical standpoint.


1. Flashing at the Parting Line

What it looks like

Thin silicone fins appear along the mold parting line or around the nipple base.

Main causes

Excessive injection pressure

Poor mold clamping force

Worn or improperly aligned mold surfaces

LSR viscosity too low for the tooling design

How to fix it

Reduce injection pressure while maintaining proper fill

Increase clamp force and verify mold alignment

Inspect and refurbish worn mold parting surfaces

Adjust LSR formulation or select a grade with slightly higher viscosity


2. Air Bubbles or Voids

What it looks like

Visible bubbles inside the nipple wall or weak, hollow sections.

Main causes

Trapped air during mold filling

Insufficient vacuum venting

Moisture contamination in raw materials

Injection speed too fast

How to fix it

Improve mold venting and vacuum efficiency

Dry all components and feeding systems thoroughly

Optimize injection speed to allow air to escape

Adjust gate design to promote smooth material flow


3. Incomplete Filling (Short Shots)

What it looks like

The nipple tip or thin sections appear underfilled or malformed.

Main causes

Injection pressure too low

Mold temperature too low

LSR curing too quickly before complete filling

Gate size too small

How to fix it

Increase injection pressure gradually

Raise mold temperature within material specifications

Slow down curing by adjusting catalyst ratio if possible

Redesign gates to improve flow into thin sections


4. Surface Tackiness or Sticky Feel

What it looks like

The nipple surface feels sticky and attracts dust after demolding.

Main causes

Incomplete curing

Incorrect A/B mixing ratio

Low mold temperature

Catalyst inhibition from contaminants

How to fix it

Verify precise A:B ratio and mixing accuracy

Increase mold temperature or curing time

Eliminate sulfur, amines, or tin-based contaminants

Use post-curing if required by the formulation


5. Poor Tear Strength at the Nipple Tip

What it looks like

The nipple tears easily during testing or early use.

Main causes

Shore hardness too low for the application

Insufficient crosslink density

Sharp mold edges creating stress concentration

Poor material selection

How to fix it

Select an LSR grade designed for high tear resistance

Optimize curing conditions for full crosslinking

Polish and round critical mold areas

Balance softness and mechanical strength carefully


6. Demolding Deformation

What it looks like

The nipple stretches, collapses, or deforms during ejection.

Main causes

Part removed before full curing

Excessively soft LSR formulation

Aggressive demolding speed

How to fix it

Extend curing time slightly

Use an LSR grade with better green strength

Optimize demolding automation speed and angles


7. Color Inconsistency or Streaking

What it looks like

Uneven color distribution or streaks across the nipple surface.

Main causes

Poor pigment dispersion

Inadequate mixing of LSR components

Inconsistent injection parameters

How to fix it

Use pre-dispersed, food-grade color masterbatches

Improve static mixer performance

Stabilize injection speed and pressure


Final Thoughts

LSR baby nipple molding demands tight control over materials, tooling, and processing conditions. Most defects trace back to a small number of variables-mixing accuracy, mold design, temperature control, and material selection.

When manufacturers understand how each defect forms and address the root cause directly, they can achieve consistent quality, longer mold life, and safer products that meet global infant-care standards.

Send Inquiry